  • Aluminum Degreaser Powder - 2lb Makes 3 Gallons

    Aluminum Degreaser Powder - 2lb Makes 3 Gallons

    This special degreaser for Aluminum quickly cleans any aluminum alloy without etching. Mix 2 lbs of cleaner with 3 gallons of distilled water in a stainless steel container. Heat to 130 deg F on a hotplate. Immerse aluminum parts for 3-10 minutes prior...
    $34.78
    Add to Cart
  • ANODIZE & CHROME  STRIPPER - 8 OZ

    ANODIZE & CHROME STRIPPER - 8 OZ

    8 fl oz of stripping solution. To strip anodize, immerse parts for 5-30 minutes. To strip chrome, use a stainless steel wand and 12V DC. Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1...
    $8.84
    Add to Cart
  • ANODIZE & CHROME STRIPPER

    ANODIZE & CHROME STRIPPER

    Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains Hazardous Goods. Shipping restrictions apply. Ground shipping...
    $62.61
    Add to Cart
  • ANODIZE FUME SUPPRESSANT

    ANODIZE FUME SUPPRESSANT

    2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses.  Re-dose when fumes are detected. DO NOT OVERDOSE.  
    $17.07
    Add to Cart
  • Anodizing Sealant - 1 lb

    Anodizing Sealant - 1 lb

    Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes.
    $36.67
    Add to Cart
  • Deoxidizer/Desmut - 1 Quart

    Deoxidizer/Desmut - 1 Quart

    1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA...
    $27.19
    Add to Cart
  • GP PLATE - 20" x 20" x 1/32"

    GP PLATE - 20" x 20" x 1/32"

    "General Purpose" plates. Ideal for larger anodizing systems (use as cathodes), or stripping tanks. Lead sheet is 1/32" thick. Can also be used as an anode when chrome plating.
    $68.30
    Add to Cart
  • GP PLATES 8 x 8

    GP PLATES 8 x 8

    "General Purpose" plates. Ideal for larger anodizing systems (use as cathodes), or stripping tanks. Lead sheet is 1/32" thick. Can also be used as an anode when chrome plating.
    $17.07
    Add to Cart
  • MASK IT MASKING LACQUER - 8OZ

    MASK IT MASKING LACQUER - 8OZ

    Caswell Mask It Masking Lacquer is an optically Blue Tinted acid resistant, peelable coating used where an acid resistant protective coating is required. Various applications include: protection of surfaces during fabrication and milling operations,...
    $13.90