null
Additional Items Required
Get Our Plating Manual

PTFE Plating Kits

  • PTFE Dispersion Powder - 120g (4oz)

    For use with our One-Plate® 1 Electroless Nickel System. Add 23 grams PFTE powder to each gallon of new One-Plate® 1 solution. Note that the bottle may appear half full. Product is shipped by weight,...
    $39.10
    Add to Cart
  • PTFE Dispersion Powder - 240g (8oz)

    For use with our One-Plate® 1 Electroless Nickel System. Add 23 grams PFTE powder to each gallon of new One-Plate® 1 solution. Note that the bottle may appear half full. Product is shipped by weight,...
    $67.85
    Add to Cart
  • PTFE Dispersion Powder - 60g (2oz)

    For use with our One-Plate® 1 Electroless Nickel System Add 23 grams PFTE powder to each gallon of new One-Plate® 1 solution. Note that the bottle may appear half full. Product is shipped by weight,...
    $21.85
    Add to Cart