Quick view Caswell sku: STRP5 ANODIZE & CHROME STRIPPER - 8 OZ MSRP: Now: $8.84 Add to Cart Compare Quick view Caswell sku: ALDEOX28 Deoxidizer/Desmut - 1 Quart MSRP: Now: $27.19 Add to Cart Compare Quick view Caswell sku: ALSE22 Anodizing Sealant - 1 lb MSRP: Now: $36.67 Add to Cart Compare Quick view Caswell sku: TW21 2 X 3 FOOT TITANIUM WIRES MSRP: Now: $13.90 Add to Cart Compare Quick view Caswell sku: ANFUM10 ANODIZE FUME SUPPRESSANT MSRP: Now: $17.07 Add to Cart Compare Quick view Caswell sku: ANSTP1G ANODIZE & CHROME STRIPPER MSRP: Now: $62.61 Add to Cart Compare Quick view Caswell sku: CWHEEL ANODIZING COLOR WHEEL MSRP: Now: $5.30 Add to Cart Compare Quick view Caswell sku: DYERB9 RED BORDEAUX 2R ANODIZING DYE - 4OZ MSRP: Now: $16.18 Add to Cart Compare Quick view Caswell sku: ADSKIT Anodizing Dye Sample Kit MSRP: Now: $85.00 Add to Cart Compare Quick view Caswell sku: AN2 Deluxe Anodizing Kit - Includes 30 Amp Rectifier MSRP: Now: $1,326.97 Choose Options Compare Quick view Caswell sku: AN1 Standard Anodizing Kit MSRP: Now: $662.85 Choose Options Compare Quick view ANODIZE & CHROME STRIPPER - 8 OZ 8 fl oz of stripping solution. To strip anodize, immerse parts for 5-30 minutes. To strip chrome, use a stainless steel wand and 12V DC. Contains Hazardous Goods. Shipping restrictions apply. Ground... MSRP: Now: $8.84 Add to Cart Compare Quick view Deoxidizer/Desmut - 1 Quart 1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions... MSRP: Now: $27.19 Add to Cart Compare Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Caswell sku: ALDEOX28 Deoxidizer/Desmut - 1 Quart MSRP: Now: $27.19 Add to Cart Compare Quick view Caswell sku: ALSE22 Anodizing Sealant - 1 lb MSRP: Now: $36.67 Add to Cart Compare Quick view Caswell sku: TW21 2 X 3 FOOT TITANIUM WIRES MSRP: Now: $13.90 Add to Cart Compare Quick view Caswell sku: ANFUM10 ANODIZE FUME SUPPRESSANT MSRP: Now: $17.07 Add to Cart Compare Quick view Caswell sku: ANSTP1G ANODIZE & CHROME STRIPPER MSRP: Now: $62.61 Add to Cart Compare Quick view Caswell sku: CWHEEL ANODIZING COLOR WHEEL MSRP: Now: $5.30 Add to Cart Compare Quick view Caswell sku: DYERB9 RED BORDEAUX 2R ANODIZING DYE - 4OZ MSRP: Now: $16.18 Add to Cart Compare Quick view Caswell sku: ADSKIT Anodizing Dye Sample Kit MSRP: Now: $85.00 Add to Cart Compare Quick view Caswell sku: AN2 Deluxe Anodizing Kit - Includes 30 Amp Rectifier MSRP: Now: $1,326.97 Choose Options Compare Quick view Caswell sku: AN1 Standard Anodizing Kit MSRP: Now: $662.85 Choose Options Compare Quick view ANODIZE & CHROME STRIPPER - 8 OZ 8 fl oz of stripping solution. To strip anodize, immerse parts for 5-30 minutes. To strip chrome, use a stainless steel wand and 12V DC. Contains Hazardous Goods. Shipping restrictions apply. Ground... MSRP: Now: $8.84 Add to Cart Compare Quick view Deoxidizer/Desmut - 1 Quart 1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions... MSRP: Now: $27.19 Add to Cart Compare Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Caswell sku: ALSE22 Anodizing Sealant - 1 lb MSRP: Now: $36.67 Add to Cart Compare Quick view Caswell sku: TW21 2 X 3 FOOT TITANIUM WIRES MSRP: Now: $13.90 Add to Cart Compare Quick view Caswell sku: ANFUM10 ANODIZE FUME SUPPRESSANT MSRP: Now: $17.07 Add to Cart Compare Quick view Caswell sku: ANSTP1G ANODIZE & CHROME STRIPPER MSRP: Now: $62.61 Add to Cart Compare Quick view Caswell sku: CWHEEL ANODIZING COLOR WHEEL MSRP: Now: $5.30 Add to Cart Compare Quick view Caswell sku: DYERB9 RED BORDEAUX 2R ANODIZING DYE - 4OZ MSRP: Now: $16.18 Add to Cart Compare Quick view Caswell sku: ADSKIT Anodizing Dye Sample Kit MSRP: Now: $85.00 Add to Cart Compare Quick view Caswell sku: AN2 Deluxe Anodizing Kit - Includes 30 Amp Rectifier MSRP: Now: $1,326.97 Choose Options Compare Quick view Caswell sku: AN1 Standard Anodizing Kit MSRP: Now: $662.85 Choose Options Compare Quick view ANODIZE & CHROME STRIPPER - 8 OZ 8 fl oz of stripping solution. To strip anodize, immerse parts for 5-30 minutes. To strip chrome, use a stainless steel wand and 12V DC. Contains Hazardous Goods. Shipping restrictions apply. Ground... MSRP: Now: $8.84 Add to Cart Compare Quick view Deoxidizer/Desmut - 1 Quart 1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions... MSRP: Now: $27.19 Add to Cart Compare Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Caswell sku: TW21 2 X 3 FOOT TITANIUM WIRES MSRP: Now: $13.90 Add to Cart Compare Quick view Caswell sku: ANFUM10 ANODIZE FUME SUPPRESSANT MSRP: Now: $17.07 Add to Cart Compare Quick view Caswell sku: ANSTP1G ANODIZE & CHROME STRIPPER MSRP: Now: $62.61 Add to Cart Compare Quick view Caswell sku: CWHEEL ANODIZING COLOR WHEEL MSRP: Now: $5.30 Add to Cart Compare Quick view Caswell sku: DYERB9 RED BORDEAUX 2R ANODIZING DYE - 4OZ MSRP: Now: $16.18 Add to Cart Compare Quick view Caswell sku: ADSKIT Anodizing Dye Sample Kit MSRP: Now: $85.00 Add to Cart Compare Quick view Caswell sku: AN2 Deluxe Anodizing Kit - Includes 30 Amp Rectifier MSRP: Now: $1,326.97 Choose Options Compare Quick view Caswell sku: AN1 Standard Anodizing Kit MSRP: Now: $662.85 Choose Options Compare Quick view ANODIZE & CHROME STRIPPER - 8 OZ 8 fl oz of stripping solution. To strip anodize, immerse parts for 5-30 minutes. To strip chrome, use a stainless steel wand and 12V DC. Contains Hazardous Goods. Shipping restrictions apply. Ground... MSRP: Now: $8.84 Add to Cart Compare Quick view Deoxidizer/Desmut - 1 Quart 1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions... MSRP: Now: $27.19 Add to Cart Compare Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Caswell sku: ANFUM10 ANODIZE FUME SUPPRESSANT MSRP: Now: $17.07 Add to Cart Compare Quick view Caswell sku: ANSTP1G ANODIZE & CHROME STRIPPER MSRP: Now: $62.61 Add to Cart Compare Quick view Caswell sku: CWHEEL ANODIZING COLOR WHEEL MSRP: Now: $5.30 Add to Cart Compare Quick view Caswell sku: DYERB9 RED BORDEAUX 2R ANODIZING DYE - 4OZ MSRP: Now: $16.18 Add to Cart Compare Quick view Caswell sku: ADSKIT Anodizing Dye Sample Kit MSRP: Now: $85.00 Add to Cart Compare Quick view Caswell sku: AN2 Deluxe Anodizing Kit - Includes 30 Amp Rectifier MSRP: Now: $1,326.97 Choose Options Compare Quick view Caswell sku: AN1 Standard Anodizing Kit MSRP: Now: $662.85 Choose Options Compare Quick view ANODIZE & CHROME STRIPPER - 8 OZ 8 fl oz of stripping solution. To strip anodize, immerse parts for 5-30 minutes. To strip chrome, use a stainless steel wand and 12V DC. Contains Hazardous Goods. Shipping restrictions apply. Ground... MSRP: Now: $8.84 Add to Cart Compare Quick view Deoxidizer/Desmut - 1 Quart 1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions... MSRP: Now: $27.19 Add to Cart Compare Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Caswell sku: ANSTP1G ANODIZE & CHROME STRIPPER MSRP: Now: $62.61 Add to Cart Compare Quick view Caswell sku: CWHEEL ANODIZING COLOR WHEEL MSRP: Now: $5.30 Add to Cart Compare Quick view Caswell sku: DYERB9 RED BORDEAUX 2R ANODIZING DYE - 4OZ MSRP: Now: $16.18 Add to Cart Compare Quick view Caswell sku: ADSKIT Anodizing Dye Sample Kit MSRP: Now: $85.00 Add to Cart Compare Quick view Caswell sku: AN2 Deluxe Anodizing Kit - Includes 30 Amp Rectifier MSRP: Now: $1,326.97 Choose Options Compare Quick view Caswell sku: AN1 Standard Anodizing Kit MSRP: Now: $662.85 Choose Options Compare Quick view ANODIZE & CHROME STRIPPER - 8 OZ 8 fl oz of stripping solution. To strip anodize, immerse parts for 5-30 minutes. To strip chrome, use a stainless steel wand and 12V DC. Contains Hazardous Goods. Shipping restrictions apply. Ground... MSRP: Now: $8.84 Add to Cart Compare Quick view Deoxidizer/Desmut - 1 Quart 1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions... MSRP: Now: $27.19 Add to Cart Compare Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Caswell sku: CWHEEL ANODIZING COLOR WHEEL MSRP: Now: $5.30 Add to Cart Compare Quick view Caswell sku: DYERB9 RED BORDEAUX 2R ANODIZING DYE - 4OZ MSRP: Now: $16.18 Add to Cart Compare Quick view Caswell sku: ADSKIT Anodizing Dye Sample Kit MSRP: Now: $85.00 Add to Cart Compare Quick view Caswell sku: AN2 Deluxe Anodizing Kit - Includes 30 Amp Rectifier MSRP: Now: $1,326.97 Choose Options Compare Quick view Caswell sku: AN1 Standard Anodizing Kit MSRP: Now: $662.85 Choose Options Compare Quick view ANODIZE & CHROME STRIPPER - 8 OZ 8 fl oz of stripping solution. To strip anodize, immerse parts for 5-30 minutes. To strip chrome, use a stainless steel wand and 12V DC. Contains Hazardous Goods. Shipping restrictions apply. Ground... MSRP: Now: $8.84 Add to Cart Compare Quick view Deoxidizer/Desmut - 1 Quart 1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions... MSRP: Now: $27.19 Add to Cart Compare Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Caswell sku: DYERB9 RED BORDEAUX 2R ANODIZING DYE - 4OZ MSRP: Now: $16.18 Add to Cart Compare Quick view Caswell sku: ADSKIT Anodizing Dye Sample Kit MSRP: Now: $85.00 Add to Cart Compare Quick view Caswell sku: AN2 Deluxe Anodizing Kit - Includes 30 Amp Rectifier MSRP: Now: $1,326.97 Choose Options Compare Quick view Caswell sku: AN1 Standard Anodizing Kit MSRP: Now: $662.85 Choose Options Compare Quick view ANODIZE & CHROME STRIPPER - 8 OZ 8 fl oz of stripping solution. To strip anodize, immerse parts for 5-30 minutes. To strip chrome, use a stainless steel wand and 12V DC. Contains Hazardous Goods. Shipping restrictions apply. Ground... MSRP: Now: $8.84 Add to Cart Compare Quick view Deoxidizer/Desmut - 1 Quart 1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions... MSRP: Now: $27.19 Add to Cart Compare Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Caswell sku: ADSKIT Anodizing Dye Sample Kit MSRP: Now: $85.00 Add to Cart Compare Quick view Caswell sku: AN2 Deluxe Anodizing Kit - Includes 30 Amp Rectifier MSRP: Now: $1,326.97 Choose Options Compare Quick view Caswell sku: AN1 Standard Anodizing Kit MSRP: Now: $662.85 Choose Options Compare Quick view ANODIZE & CHROME STRIPPER - 8 OZ 8 fl oz of stripping solution. To strip anodize, immerse parts for 5-30 minutes. To strip chrome, use a stainless steel wand and 12V DC. Contains Hazardous Goods. Shipping restrictions apply. Ground... MSRP: Now: $8.84 Add to Cart Compare Quick view Deoxidizer/Desmut - 1 Quart 1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions... MSRP: Now: $27.19 Add to Cart Compare Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Caswell sku: AN2 Deluxe Anodizing Kit - Includes 30 Amp Rectifier MSRP: Now: $1,326.97 Choose Options Compare Quick view Caswell sku: AN1 Standard Anodizing Kit MSRP: Now: $662.85 Choose Options Compare Quick view ANODIZE & CHROME STRIPPER - 8 OZ 8 fl oz of stripping solution. To strip anodize, immerse parts for 5-30 minutes. To strip chrome, use a stainless steel wand and 12V DC. Contains Hazardous Goods. Shipping restrictions apply. Ground... MSRP: Now: $8.84 Add to Cart Compare Quick view Deoxidizer/Desmut - 1 Quart 1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions... MSRP: Now: $27.19 Add to Cart Compare Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Caswell sku: AN1 Standard Anodizing Kit MSRP: Now: $662.85 Choose Options Compare Quick view ANODIZE & CHROME STRIPPER - 8 OZ 8 fl oz of stripping solution. To strip anodize, immerse parts for 5-30 minutes. To strip chrome, use a stainless steel wand and 12V DC. Contains Hazardous Goods. Shipping restrictions apply. Ground... MSRP: Now: $8.84 Add to Cart Compare Quick view Deoxidizer/Desmut - 1 Quart 1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions... MSRP: Now: $27.19 Add to Cart Compare Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view ANODIZE & CHROME STRIPPER - 8 OZ 8 fl oz of stripping solution. To strip anodize, immerse parts for 5-30 minutes. To strip chrome, use a stainless steel wand and 12V DC. Contains Hazardous Goods. Shipping restrictions apply. Ground... MSRP: Now: $8.84 Add to Cart Compare Quick view Deoxidizer/Desmut - 1 Quart 1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions... MSRP: Now: $27.19 Add to Cart Compare Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Deoxidizer/Desmut - 1 Quart 1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes. Contains Hazardous Goods. Shipping restrictions... MSRP: Now: $27.19 Add to Cart Compare Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Anodizing Sealant - 1 lb Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes. MSRP: Now: $36.67 Add to Cart Compare Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view 2 X 3 FOOT TITANIUM WIRES 2 x 3 foot long Titanium Wires, for hanging parts into the anodizing tank. MSRP: Now: $13.90 Add to Cart Compare Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view ANODIZE FUME SUPPRESSANT 2 fl oz bottle Add One Teaspoon fume suppressant to a 5 gallon anodizing bath. Each 2oz bottle contains 10 doses. Re-dose when fumes are detected. DO NOT OVERDOSE. MSRP: Now: $17.07 Add to Cart Compare Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view ANODIZE & CHROME STRIPPER Anodize & Chrome Stripper is a super fast commercial grade stripper. It outperforms all others in speed and quality. Does not attack the aluminum. 1 lb of powder makes 3 gallons. Contains... MSRP: Now: $62.61 Add to Cart Compare Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view ANODIZING COLOR WHEEL The color wheel helps the anodizer, or painter, to decide which colors to mix to achieve their desired results. MSRP: Now: $5.30 Add to Cart Compare Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view RED BORDEAUX 2R ANODIZING DYE - 4OZ 4oz Dye - Makes 2 Gallons MSRP: Now: $16.18 Add to Cart Compare Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Anodizing Dye Sample Kit Orange 3A, Deep Red, Yellow 4A, Green AEN, Blue 4A, Violet 3D 4oz bottles of each - Makes 2 Gals of Each Color MSRP: Now: $85.00 Add to Cart Compare Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Deluxe Anodizing Kit - Includes 30 Amp Rectifier A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means – Inexpensive... MSRP: Now: $1,326.97 Choose Options Compare Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected × OK
Quick view Standard Anodizing Kit A revolution in Small Scale Anodizing! Provides a durable anodized surface - which can easily be dyed. Simple to operate - Predictable consistent results Low Current Density means –... MSRP: Now: $662.85 Choose Options Compare Previous 1 2 3 4 5 6 Previous 1 2 3 4 5 6 Compare Selected