Product Description
Color steel and stainless steel parts by heat treating and oil quenching
Possible colors include yellows, browns, purples and blues.
Our Heat Coloring Kit Includes Casweld™ Keep Kool™ Putty, which prevents heat from travelling up your pliers or other part holder and burning you.
With the use of a blowtorch or gas burner (not included), steel and stainless parts can be colored by heating up to different temperatures:
On Stainless, color changes start at approx 550 deg F for a pale yellow and continue to change until a dark blue will occur at approx 1100 deg F.
On mild steel, color changes start at 350 deg F and continue through 750 deg F.
Never heat color knife blades or other tempered steels, as this will damage them.
Rainbow/Prism effects can be achieved by heating up different areas of the part to different temperatues. This can be achieved by using the Keep Kool™ to "mask off" areas of the part to prevent them from heating. Patterns are limited only by your imagination.
The Kit Includes:
- 1 x 2lb Tub Casweld™ Keep Kool™ Putty
- 1 x Quart Quenching Oil
- 1 x Quart Liquid Degreaser
- 2 x Cans For Degreasing and Quenching
- Instructions with color chart
Instructions For Steel & Stainless Steel Parts
- Parts Must Be Polished or sanded first
- Never heat color knife blades or previously heat colored or tempered parts
- Part must be perfectly clean and dry before heating (no fingerprints, dust, oils)
- If using a blowtorch, make sure you have lots of fuel. Once you start the process, you can€™t stop
- Different alloys of steel will have slightly different colors
- We recommend practicing technique and timing on scrap parts first
Steps:
- Remove all combustibles, paper, rags etc from the heating and quenching area
- Place the Quenching Oil outside, or in a well ventilated area
- Form a large blob of The Keep Kool Putty around your part holder, pliers etc to prevent the holder from heating up and burning your hand.
- NOTE You can also use the putty to mask off certain areas to create patterns. The metal under the putty will not heat up.
- Fully degrease the part in the degreasing solution
- Avoiding touching the part with your bare fingers, attach to your holder or pliers etc
- Begin heating the part, rotating the part over the flame to heat evenly.
- After the color begins to change, back off the heat a little and watch the part closely. It will progress through the colors quickly.
- Once the correct color is achieved, quench the part in the oil. Do not allow the part to touch the sides or bottom of the container.
- Once it has cooled down, remove it from the oil and allow to dry for approx. 20 mins
- Wipe off excess oil and enjoy your new colored part.
 
            Safety Information
Product Videos
Product Reviews
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.
 
 
             
       
             
                   
           
                   
           
                   
           
          