Product Description
Jeep Wrangler® owners know that the exposed bolts on their vehicles will rust over time (mine only took 2 weeks after develiery). The factory Black Oxide finish wears off, exposing the steel bolts to the elements.
Door hinge bolts seem to be especially vulnerable because they are frequently removed and re-installed when taking the doors on and off.
Our restoration kit makes bringing these bolts back to their factory finish easy and inexpensive.
First, dip the parts in the bottle of Evapo-Rust solution to remove any surface rust. Leave the parts in the solution for 10-20 minutes.
Rinse the parts in water, then dip in the Black Oxide solution for approx 2 minutes.
Remove the parts and dip in the Caswell Sealer for approx 5 minutes. Allow to air dry.
Works on any steel bolt or nut, any vehicle. Not for Stainless Steel.
Jeep Wrangler is a registered trademark of FCA US LLC. This product is not endorsed by FCA US LCC.
                Recommended Skill Level
                    Beginner level products can and should be used by anybody, including those who consider themselves not crafty, handy or hands on. Most beginner level products can be used out of the box and can expect results within minutes. It is always important to read the product instructions and description on the web site before use, for example, nearly all of our plating kits require a polished and clean surface before plating.
Safety Information
Hazardous Shipping Info
GHS Info
SDS
Product Videos
Product Reviews
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
 - Copper Wire to hang items
 - Small amount of electrical wire to make connections
 - DC Power Supply - Included In Some Kits. Check kit contents on web site
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
 - 1 Gal Battery Acid
 - Dyes (if desired)
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.