Product Description
Black Oxide Activator
Product does not perform blackening. It is an activator for use before blackening.
Certain hardened or specialized steels can prove challenging to blacken with our Black Oxide solution, only blackening to a grey color.
Our Black Oxide Activator enhances the color and depth of the blackened finish on these alloys.
Mix One Part Activator With Nine Parts Distilled Water in a plastic container.
Immerse cleaned steel parts in the activator for 2-5 minutes, rinse, then proceed to blackening.
Can be used at room temperature or heated to 120 deg F for an even greater activating effect.
For Steel Parts Only - Not Stainless Steel or Iron.
            Safety Information
GHS Info
SDS
Product Videos
Product Reviews
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
 - Copper Wire to hang items
 - Small amount of electrical wire to make connections
 - DC Power Supply - Included In Some Kits. Check kit contents on web site
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
 - 1 Gal Battery Acid
 - Dyes (if desired)
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.