Product Description
Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes.
Safety Information
GHS Info
SDS
Product Videos
Product Reviews
24 Reviews Hide Reviews Show Reviews
-
Great
Works well to seal the parts
-
Works great!
Very affordable and great working sealant! Thanks Caswells!
-
Anodizing Sealant works well
Have only used it once so far, but it appears to have done a great job.
-
sealant
Prompt service no complaints
-
sealant
Prompt service no complaints
-
easy to use sealer
Haven't been anodizing long, but this sealer is easy to mix/use and seems to do what it's supposed to. Just be sure to follow instructions included with it to get optimal results.
-
Good products
Good products and fast shipping
-
fast shipping and a great product
Fast shipping and a great product.
-
Thanks for the prompt service
Very fast transaction and a great product
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.