Product Description
Nickel Acetate based sealer. Use at the rate of 1 oz to 1 gal of water. This 1 lb bag makes 16 gallons. Bath life is 14-60 days, depending on use. Heat to 210 deg F, and seal for 5-30 minutes.
Safety Information
GHS Info
SDS
Product Videos
Product Reviews
24 Reviews Hide Reviews Show Reviews
-
A+
Seals just like it should make sure you get the correct heater from Caswell.
-
Seals in the Color
Great for sealing in that just right color
-
Make it last
Lasts much longer and better if sealed with this product.
-
seals
Worked good for me, found 15 mins at 200 degrees was plenty of time.
-
Ya need it too!
Yes you can seal your anodized parts by just boiling them in water, but is it good enough? I don't care to take that chance. I'll buy this over and over and over again. It seals my parts and protects them.. that's all I care about
-
Anodize Sealant
Works as described with very little color bleed. It even smells ok.
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.