Product Description
IRIDESCENT YELLOW CHROMATE
After preparing the part to accept the process, the part is simply dipped into a solution for a few minutes. The zinc & the chromate react to form the new colors. To improve those older zinc (pot metal) castings, plate with a fresh zinc plate before chromating.
The Yellow Chromate is a yellow/bronze iridescent finish on plated cadmium and zinc. Liquid concentrate is used at 0.5% to 3% by volume in water at 65° to 90°F. The finish has outstanding resistance to salt spray, greatly surpasses the normal 96 hour salt spray resistance specified for yellow chromates on zinc. It will withstand up to 200 hours salt spray. The deposit is a pleasing finish in itself. It is an excellent base for paint. The finish may be dyed to various colors.
4 fl oz bottle - makes 4 gallons
Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.
![]()  |      ![]()  |      ![]()  |      ![]()  |    
            Safety Information
Hazardous Shipping Info
GHS Info
SDS
Product Videos
Product Reviews
27 Reviews Hide Reviews Show Reviews
- 
                
The ideal finish
the yellow chromate is one of my favorite way to finish off the plating process. the color is bright and looks absolutely amazing. this is a must if you plating or restoring the old factory look of parts and bolts.
 - 
                
Yellow chromate
I’m no metal finisher, but I needed some car parts plated. This yellow really looks nice and this was on my first try. Still learning and I can only expect my results to get better.
 - 
                
Good product, temperamental process
Like all Caswell chemicals, this is a high quality product. I wouldn't recommend the yellow chromate for beginners though. If you're new to plating like I am, start with the blue. It's a bit more forgiving. It seems there's a bit of a learning curve to getting a good finish with yellow. I still gave 5 stars, because it's a reflection on my plating skills and not the product. I may try again with the yellow once I have a bit more experience under my belt.
 - 
                
Perfect Color
This color replicates the original finish on Rochester Quadrajets perfectly. The shade of yellow is right on. You can vary the darkness by increasing or decreasing your dunk time. The iridescence gives GM carburetors an authentic look.
 - 
                
super results
I hate rust and on my 74 Ranchero the factory did no plating on any metal parts under the dash ASM. So I needed to plate and chromate my car parts and came out looking great. If you get the zinc right the chromate will be right. Did carburetor as well and came out looking just like what they show. Very happy!
 - 
                
great
just what the doctor prescribed...
 - 
                
All parts are 1st. class
Never had any issue,s with this brightner. Best stuff on market. Always buy my plating parts from them.If you need it they have it. Packages are done first class also, Glad to be a purchaser.
 - 
                
Yellow Chromate
Does a very nice job.
 - 
                
Worked great for that cadmium look
The yellow chromate worked graet on my zinc plated parts in giving them the cadmium look. Just dip in solution for about a minute, wash with water and you are done.
 
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
 - Copper Wire to hang items
 - Small amount of electrical wire to make connections
 - DC Power Supply - Included In Some Kits. Check kit contents on web site
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
 - 1 Gal Battery Acid
 - Dyes (if desired)
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.
            
            
            
          
          
      