Product Description
IRIDESCENT YELLOW CHROMATE
After preparing the part to accept the process, the part is simply dipped into a solution for a few minutes. The zinc & the chromate react to form the new colors. To improve those older zinc (pot metal) castings, plate with a fresh zinc plate before chromating.
The Yellow Chromate is a yellow/bronze iridescent finish on plated cadmium and zinc. Liquid concentrate is used at 0.5% to 3% by volume in water at 65° to 90°F. The finish has outstanding resistance to salt spray, greatly surpasses the normal 96 hour salt spray resistance specified for yellow chromates on zinc. It will withstand up to 200 hours salt spray. The deposit is a pleasing finish in itself. It is an excellent base for paint. The finish may be dyed to various colors.
4 fl oz bottle - makes 4 gallons
Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.
![]() | ![]() | ![]() | ![]() |
Safety Information
Hazardous Shipping Info
GHS Info
SDS
Product Videos
Product Reviews
27 Reviews Hide Reviews Show Reviews
-
Customer service
I got great customer service when I called with questions. The man I spoke with was quite knowledgeable. I would buy from them again.
-
cad plating Porsche parts
the plating looks great
-
Yellow Chromate
Product yields superior results. Easy to use.
-
Excellent color
the Color is Excellent ,adding brightener is a trial and experimentation process with excellent results
-
Amazing Results
I have been zinc plating for some time and bought the Yellow Chromate for my car project and at first I didn't heat the Chromic Acid (66F). It came out looking very variegated and I it kind washed off when I spray rinsed. I rasied the temp to 80F and the colors and depth have improved.
-
Product works!!! Service was super.
Highly recommend these folks for any plating needs.
-
Fast delivery
This is a good product, been using it for years.
-
Great Cad Results
Results look just like Cad parts
-
luv the color!
with trial and errors this can produce nice looking parts.
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.