Product Description
Easily spot blacken steel (not stainless) or iron. Simply apply the black oxide gel where you want the blackening to occur. The gel keeps the blackener in place. Leave it on the part for 1-3 minutes and rinse off. Seal with Caswell Sealer for a dry finish.
Black Oxide Gel Kit Includes:
- 4 fl oz Black Oxide Concentrate Gel (covers approx 2 sq ft)
 - 4 fl oz Caswell Sealer
 - Disposable Vinyl Gloves
 
Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.
                
                    
                Recommended Skill Level
                    Beginner level products can and should be used by anybody, including those who consider themselves not crafty, handy or hands on. Most beginner level products can be used out of the box and can expect results within minutes. It is always important to read the product instructions and description on the web site before use, for example, nearly all of our plating kits require a polished and clean surface before plating.
Safety Information
Hazardous Shipping Info
GHS Info
SDS
Product Videos
Product Reviews
20 Reviews Hide Reviews Show Reviews
- 
                
Works good to blue steel parts
I've used other competing cold blues and this works very nicely. Any gel oxidation applied the right way can get you nice streak-free color. Rub the color in smooth and apply with spots of torch heat.
 - 
                
Works OK until it dries out and turns solid
When I first purchased the gel it worked as advertised but I use it in small quantities to just blacken small parts by using a Q-tip dipped into the bottle and then capping it. After a half dozen uses and consuming about maybe 15% of the gel content in the bottle, it's dried to the point where it's almost like hard wax and unusable as the active ingredient apparently evaporates quickly when you open the bottle. I can see a squeeze container like a tube working better for the gel than the small bottle which allows the volatile solution to quickly evaporate. The only way I see being able to use the full gel contents is if it's consumed in a couple uses, not for small quantity use multiple times.
 - 
                
Worked well
This worked very well - but - was not the right product for what I was trying to do. Wound up having the rods powder coated. I have used it on several other small projects and it was fine. I will reorder.
 - 
                
Easy to use and smooth finish.
Application was a breeze. The sealer leaves a satin finish that is durable and easy to clean.
 - 
                
Works fine on carbon steel.
I tried this product on an Ed Brown Stainless Steel Ambidextrous thumb safety and it would not work at all. I also tried it on a Kimber Eclipse Stainless Steel and it also would not work. However, when I applied it to several Smith and Alexander magwells, that are carbon or blue steel parts, it worked fine. I also tried it on Kimber MIM parts, which are plastic metal injection molded, it would not work on these either. But, I was very pleased with the outcome on the carbon or blue steel parts. It seems to stay far better than cold blueing.
 - 
                
Used product to blacken armour
took 2 coats to fully blacken large surface, metal may not have been quite clean enough. Would work great for small pieces or touch ups.
 - 
                
Works well enough
I used this on two knives I made by hand and to finish an axe head I reground. Finish was inconsistent and blotchy on one of the knives but worked well the other two times. Perhaps the knife wasn't clean enough?
 - 
                
Black Oxide gel
I am happy with the oxide kit and it works fast and makes a black or greyish black finish on steel.If there is a weak spot ,it is easy to touch up to get a consistent color.Once the piece is sealed,it looks even blacker.It is also ideal for making antiqued look if desired.
 - 
                
Works exactly as advertised
Clean the part with dish soap and water, coat it with the blackener, rinse it off and coat it with the sealer. It worked great for the small part that I used it on, looks like a commercial product, a nice flat black finish.
 
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
 - Copper Wire to hang items
 - Small amount of electrical wire to make connections
 - DC Power Supply - Included In Some Kits. Check kit contents on web site
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
 - 1 Gal Battery Acid
 - Dyes (if desired)
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.