Procedure for Obtaining Dyed Anodize
Anodize the aluminum at 60-75°F for 90 minutes at 4.5 amps per sq foot or 0.03 amps per sq inch. Use our Anodizing Kit.
After thorough rinsing, immerse the part in the dye at a temperature of 140°F for 15 minutes.
Finally, seal by hanging the part in a sealer bath for 15 minutes.
All dyes are fully ROHS compliant.

Safety Information
GHS Info

SDS
Product Videos
Product Reviews
7 Reviews Hide Reviews Show Reviews
-
Great color.
Very vibrant color. Higly recommended.
-
Awesome Violet Color
Good dye uptake. I left my parts in the dye at 140° for the maximum time with a oxide layer of .7 mil, final color was pretty close to what is shown. Surface finish plays a role in the final color also. Overall, I really like this color. It looks great.
-
Amazing
Just a fantastic purple/violet. Amazing saturation. It takes very fast at 140 degrees, but depending on the time it can go from a neon color to deep and rich. My favorite color so far.
-
Thanks for the prompt service
Fast shipping!! Thank you so much!!
-
alright
Turned out a little darker for me than what's shown, but great color.
-
Fantastic dye
I don't know if it's just the particular bottle I got or not, but this dye is fantastic. I don't have to leave my parts in very long at all for it to get the deepest most vibrant purples ever! I mean SECONDS. Not minutes. 45 seconds in this dye gives you a great purple.
-
Good dye
This dye absorbs well, and with all of caswell dyes has the ability to give lighter shades by soaking for shorter times. I love it!
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.