Product Description
Stainless Steel Blackener 370 is an acidic liquid concentrate used full strength or diluted with up to 3 parts water to blacken stainless steel at room temperature. Recommended for color coding parts and blackening engravings on stainless steels. Produces a pleasing dark gray/black finish. Seal with Caswell Sealer.Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.

            Safety Information
Hazardous Shipping Info
GHS Info
SDS
Product Videos
Product Reviews
12 Reviews Hide Reviews Show Reviews
- 
                
Great product, exactly what i needed to blacken stainless parts
I had a bunch of stainless m1 parts that had all the finish worn off. After cleaning the parts and sandblasting i wiped the blackener on and the parts turned black. It was exactly what i was looking for!
 - 
                
Blackened a M1 Garand gas cylinder perfectly, nice consistent color
Blackened a M1 Garand gas cylinder perfectly, nice consistent color
 - 
                
Great product
Great product. Very easy to use. Great value on the big bottle. Fast shipping.
 - 
                
Worked as expected - easy to use
So far have just tested to see how this worked and attempted some touch-up on a previously finished item. Very good match was achieved in the touch-up work. Blacked stainless barrel material quite well. finish seemed durable.
 - 
                
Unexpectedly Great Results
I refinished a stainless steel putter head, using minimal preparation. Cleaned the head with acetone, scrubbed it with fantastic, and then scrubbed it with distilled white vinegar (my own system obviously). Rinsed it and then dipped it in the blackener and scrubbed the head with 3M great and 3M white abrasive pads while it was submerged in the blackener, Pulled it out, rinsed, and let dry. That was it,. Amazing results for just a little work. Not perfect (not the products fault) but I will do it again and again, and try to improve my technique each time. Fun and rewarding.. A fantastic product!
 - 
                
Great Product...
Very easy to work with and leaves a nice color.
 - 
                
worked as advertized
good product and worked well. would order again.
 - 
                
Needed for golf club
Very good product
 - 
                
Works Great!
I recommend buying a pint of this for applications that require broad coverage.
 
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
 - Copper Wire to hang items
 - Small amount of electrical wire to make connections
 - DC Power Supply - Included In Some Kits. Check kit contents on web site
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
 - 1 Gal Battery Acid
 - Dyes (if desired)
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.