Product Description
NO ELECTRICITY
NO CYANIDES
NO PHOSPHATES
NO CAUSTIC AMINES
NO AMMONIA
NO FUMES
The only one-component, non-toxic, powdered, immersion nickel strippers on the market.
Removes NICKEL from steel, copper, brass and zinc diecast, silver and gold.
Caswell Inc. distributes three MetalX Nickel Strippers:
- MetalX B-9 strips nickel from steel, without etching the base metal.
- MetalX B-929 strips nickel from copper, brass, zinc diecast, pot metal, silver and gold, without etching the base metal.
- MetalX B-913 strips nickel from aluminum, without etching the base metal.
MetalX strippers will strip nickel at the rate of 2 mils per hour, and will strip 2.5-6 ounces of nickel per gallon of stripper solution. Electroless nickel will strip at the same rate, providing the phosphorous content does not exceed 5%. Higher phosphorous electroless nickel will take longer to strip.
- 2.5 lbs of MetalX stripper makes 1 gallon of stripping solution.
- Use plastic, unlined steel or stainless steel tanks
- Agitation is required during stripping
- Stripping tank must operate between 120°F-150°F. To prolong bath life, heating should be discontinued immediately after stripping is complete.
- Stainless steel or titanium heaters must be used. No quartz or ceramic heaters.
- Instruction sheet will be provided with purchase.
 
            Safety Information
GHS Info
 
			 SDS
Product Videos
Product Reviews
10 Reviews Hide Reviews Show Reviews
- 
                B9 Nickel StripperExcellent stripper! Goes a long way. I used in a ceramic crock pot. Somewhere on website or maybe in the instructions, it says not to do that, however, it worked for me several times. It removed the nickel from golf iron heads in a couple of hours. Great instructions for all Caswell products. Highly recommend this and other Caswell products. Only brand I use when it comes to chrome or nickel stripping. I also highly recommend their black oxide kit. 
- 
                Nickel stripperproduct worked just as promised. I would use it again if needing to strip nickel plating. 
- 
                Great productWorked great with the suggestions of other users 
- 
                Works great!This stuff works exactly as described. I stripped some nickel off of an old gun action and it took every spec off in just a couple hours. Another review mentioned a smell, but it wasn't this stuff, it is almost odorless. I soaked my parts in a stainless ultrasonic tank because it has a heater. When the parts were done I turned on the ultrasonic and it removed the most of the smut. I then rinsed it off with hot water. I put off this project a long time because I didn't want to mess with acids and electricity, I wish I found this sooner! 
- 
                ExcellentYour product arrived and performed as advertised. Completely satisfied. 
- 
                Worked great, thank you.Removed everything I needed removed. 
- 
                Used to strip old gunDid the job like advertised 
- 
                Used to strip old gunDid the job like advertised 
- 
                It works with patienceI used the B9 to strip a nickel plated golf club. It took much longer to strip the nickel than the guide suggested, about a week cooking 4 hours the first day and an hour each day following. The solution smells bad so I don't recommend doing it indoors. It gets clumpy and kind of messy near the end. Almost all the plating was removed, the remaining bits I sanded away. The sanding will also remove most of the soot. Overall an effective product. Will return to Caswells for more DIY projects. 
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.
 
 
             
      