Caswell Brass Plating Solution is a unique
cyanide-free alkaline brass plating system which plates
a true 70/30 yellow-green plate directly onto steel
and bright nickel plated surfaces. It can be used for
heavy brass plating which will be antiqued (oxidized
and relieved). It may also be used for decorative heavy
brass if the surface is burnished or buffed and colored
with a wheel to remove the slight haze and reveal the
true rich brass color for lamp parts, hardware and plumbing
fixtures.
To plate on zinc die cast surfaces, you must plate with Flash Copper™ first.
The system eliminates carbonates. Therefore, there is
no carbonate sludge containing cyanide to be disposed
of.
The solution may be used to tank or brush plate.
Brass tank plating requires an average current of 0.02-0.1
amps per sq. in. and operates in the range of 3-12 Volts.
Brass Plating is available on a small scale using Plug N' plate kits.
Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.