Caswell Brass Plating Solution is a unique 
  cyanide-free alkaline brass plating system which plates 
  a true 70/30 yellow-green plate directly onto steel 
  and bright nickel plated surfaces. It can be used for 
  heavy brass plating which will be antiqued (oxidized 
  and relieved). It may also be used for decorative heavy 
  brass if the surface is burnished or buffed and colored 
  with a wheel to remove the slight haze and reveal the 
  true rich brass color for lamp parts, hardware and plumbing 
  fixtures.
  
  To plate on zinc die cast surfaces, you must plate with Flash Copper™ first.
  
  The system eliminates carbonates. Therefore, there is 
  no carbonate sludge containing cyanide to be disposed 
of.
The solution may be used to tank or brush plate.
Brass tank plating requires an average current of 0.02-0.1 
  amps per sq. in. and operates in the range of 3-12 Volts. 
  
Brass Plating is available on a small scale using  Plug N' plate kits.

Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.