Product Description
Electroless Tin Plating Kit
Tin Plate Copper, Brass, Gold and Copper Based Alloys Without Power Or Heat!
Simple to use. Plates tin over copper, brass, gold and copper based alloys in seconds! No power required.
Degrease your parts and hang them into the solution from string or copper wire. Immerse in the 120F solution for 60 seconds to put a bright tin plating onto the base metal.
It couldn't be simpler!
Perfect for tin plating circuit boards, or retinning cookware.
Plates at 1/1000" per 15 mins. Bath life is approx 100 sq ft per gallon at 0.000025" thicknes.
Contains Hydrochloric Acid.
5 Gallon Kit Contains:
- 1 x 6.5 Gal Plating Tank & Lid
- 5 Gallons Electroless Tin Solution
- Instructions
- Free Technical Support
- NO HEATERS INCLUDED
Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.
![]() |
Recommended Skill Level
Beginner level products can and should be used by anybody, including those who consider themselves not crafty, handy or hands on. Most beginner level products can be used out of the box and can expect results within minutes. It is always important to read the product instructions and description on the web site before use, for example, nearly all of our plating kits require a polished and clean surface before plating.
Safety Information
Hazardous Shipping Info
GHS Info
SDS
Product Videos
Product Reviews
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.