Product Description
These professional quality anodizing dyes provide consistent, quality results. The same dyes are sold to professional anodizing shops all over the world. 4oz of dye concentrate makes 2 Gallons.
These colors are approximate. The finish will normally have a more 'metallic' look, and will vary slightly depending on the alloy and surface preparation.
Procedure for Obtaining Dyed Anodize
Anodize the aluminum at 60-75°F for 90 minutes at 4.5 amps per sq foot or 0.03 amps per sq inch. Use our Anodizing Kit.
After thorough rinsing, immerse the part in the dye at a temperature of 140°F for 15 minutes.
Finally, seal by hanging the part in a sealer bath for 15 minutes.
All dyes are fully ROHS compliant.
![This product can ship air and worldwide This product can ship air and worldwide](/content/images/airok.png)
Safety Information
GHS Info
![](/content/images/ghs_harm.png)
SDS
Product Videos
Product Reviews
3 Reviews Hide Reviews Show Reviews
-
Nice color, but pay attention to alloy
This dye makes a deep rich color, but watch the alloy. I had four parts to match. The 7075- T5 parts that came out very deep, closer to black, in 70 seconds. I had a 6061- T6 extruded part that was dyed for 20 minutes but didn't get quite as dark. No problem with the product, just something a novice such as myself may not be aware of!
-
Great dye, varying intensities possible
By varying the immersion times of this dye, you can achieve a brown "coyote" color to a deep brown, almost black intensity. Great stuff!
-
Favorite color yet!
This is my favorite color so far, very nice color!
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.