Product Description
BLUE CHROMATE

Our blue chromate concentrate produces a true blue conversion coating on zinc plated items. It is a single dip blue trivalent chromate that offers high salt spray resistance for up to 130 hours to white rust corrosion, and 160-200 hours to red rust corrosion. No additional topcoat is required to obtain this high degree of corrosion resistance. It produces a beautiful blue/clear trivalent chromate to meet automotive and all other industrial standards.
Dip zinc plated parts at room temperature for 15-40 seconds. For best results, dry with hot air (150 deg F)
Mix 1 part Blue Chromate to 4 parts Distilled Water, ie. 1 Quart Makes 1.25 Gallon Mixed
Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.
![]() | ![]() | ![]() | ![]() |
Safety Information
Hazardous Shipping Info
GHS Info
SDS
Product Videos
Product Reviews
7 Reviews Hide Reviews Show Reviews
-
this suff is cool
Looks good and last longer than I figured it would will buy again
-
simply awesome
Great buy and works well
-
man this works great
I highly recommended this to anyone
-
awesome
Really works and looks good to highly recommended to buy
-
loved it
I got this and works really well very pleased.
-
nice!
This is a must and works really good highly recommend
-
works
I use this and it really works and looks great A+
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.