Product Description
BLUE 4A ANODIZING DYE - 4OZ
These professional quality anodizing dyes provide consistent, quality results. The same dyes are sold to professional anodizing shops all over the world. 4oz of dye concentrate makes 2 Gallons.
These colors are approximate. The finish will normally have a more 'metallic' look, and will vary slightly depending on the alloy and surface preparation.
Procedure for Obtaining Dyed Anodize
Anodize the aluminum at 60-75°F for 90 minutes at 4.5 amps per sq foot or 0.03 amps per sq inch. Use our Anodizing Kit.
After thorough rinsing, immerse the part in the dye at a temperature of 140°F for 15 minutes.
Finally, seal by hanging the part in a sealer bath for 15 minutes.
All dyes are fully ROHS compliant.

Safety Information
GHS Info

SDS
Product Videos
Product Reviews
10 Reviews Hide Reviews Show Reviews
-
All in all a very good product.
It works as intended and gives my pieces a nice color. I like that I can alter the colors shade by varying the time in the dye.
-
Great Dark Blue
We use this for the dark water in a pool effect acid wash. Great color saturation.
-
Great color
great blue color.
-
Beautiful!
Very nice deep blue. Also easy to get a range of shades from light metallic to dark- almost opaque.
-
Thanks for the prompt service
Very fast transaction and a great product
-
Really nice deep blue
I use this for a midnight blue or really dark blue. Combined with just a smidgen of black
-
great color!
I like this color as is real close to the automotive colored parts i already have... I just have to play with the time.
-
great color
This dye absorbs well, and with all of caswell dyes has the ability to give lighter shades by soaking for shorter times. I love it!
-
Great Color
I have not a complaint about the color! After 7min. at 140* you get a full deep blue. I am loving this blue.
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.