Product Description
Blacken Steel & Iron Parts At Room Temperature
This new technique was developed by the commercial gun blue manufacturers as a more environmentally friendly system than the commonly used hot application. Parts requiring blackening are simply placed in the liquid at room temperature, no electrical power is required.
2.5 Gallon Kit Contains:
- 2 x 1 Pint Black Oxide Concentrate (makes 2.5 gals)
- 1 Gal Sealer - Choose Penetrating Sealer For Oily Finish or Caswell Sealer For Dry Finish
- 2 x 3.5 Gal Plastic Tanks
- Instruction Sheet
- Free Technical Support

Convenient - Easy to do in house. No waiting for heatup of blackening solution. No waiting for the unpredictable return of parts from an outside vendor. Eliminates high outside vendor costs. Retain control of production and quality. Ideal for high volume or short runs. Works especially well for blackening large volume of small parts in a rotating barrel.
Higher Productivity - Parts can be blackened in two minutes vs 15 to 30 minutes for hot oxide. Normally twice the amount of parts can be blackened in the same amount of time as with hot oxide.
Controllable - Long bath life, blackening solution may be replenished indefinitely with periodic additions of fresh concentrate.
So easy to install and use that you can now economically apply a pleasing decorative, sales-appealing black corrosion-resistant finish on parts previously left unfinished.
Versatility - Blackens cast iron, forged steels, mild steels, hardened tool steels and powdered metal parts. No white salt bleedout as is common with hot oxide.
Dimensional Control - No heat distortion. No smutty rub-off as with other room-temperature blackening processes.
Energy Cost Saving - Blackening is done at room temperature vs hot oxide blackening done at 290°F.
Safety - Blackening solution uses odorless, mild water-dilutable chemicals that require no venting vs hot oxide. No hazardous caustic chemicals with fumes that present health hazards and no spattering of hot, skin-burning chemicals.
Low Maintenance - Longer Equipment Life - No expensive pollution control equipment.
Parts Coverage - 600 to 1200 sq. ft. of surface area blackened per gallon of concentrate.
How to achieve professional results in minutes:- Thoroughly clean the part to be blackened by either sandblasting, wire brushing, wire wool abrasive cleaning, or by scrubbing in 'VIM' or 'COMET' household abrasive cleaner. Make sure you have removed all rust, paint, oil and grease.
Immerse the part in the mixed Black Oxide Solution and swirl around for between 30 seconds and 5 minutes. Alternatively, the part may simply be placed in the solution for 5 - 10 minutes. Remove the part from the solution and rinse in fresh water.
Immediately brush on or dip into the Penetrating Sealant, and allow to soak in the liquid for 5-10 minutes. Shake off any excess and allow to dry thoroughly before handling. Penetrating Sealer imparts a slightly oily feeling to the parts. If a non-oily finish is desired, do not use the Penetrating Sealer after blackening, and instead use Caswell Sealer.
Black Oxide works on steel or iron parts only and will not blacken Stainless Steel - use Stainless Steel Blackener.
Some hardened and specialized steel alloys may blacken to a deeper black finish when activated using our Black Oxide Activator.
Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.

Looking for shipping options outside the USA? Check out our NEW Mega Black Blackening Kit.
Recommended Skill Level
Beginner level products can and should be used by anybody, including those who consider themselves not crafty, handy or hands on. Most beginner level products can be used out of the box and can expect results within minutes. It is always important to read the product instructions and description on the web site before use, for example, nearly all of our plating kits require a polished and clean surface before plating.
Safety Information
Hazardous Shipping Info
GHS Info
SDS
Product Videos
Videos Hide Videos Show Videos
Product Reviews
10 Reviews Hide Reviews Show Reviews
-
Black Oxide Kit
I don't normally write reviews, but I had a great experience with Caswell so I thought I'd share. The website is great, the transaction was simple, the communication after the sale was clear, and helpful. I got shipping updates quickly, and my order shipped the same day. I received the order faster than I expected. The Black Oxide system is amazing. I have used other company's products in the past, but Caswell's black oxide system works beautifully. Just following the included instructions, I was able to get excellent, professional looking results. I will say that you should give yourself some time and don't get in a hurry. The initial surface prep is key to a consistent finish. I setup an assembly-line type procedure with timers to ensure that all my parts came out with the same even finish. I also let the sealer dry for several days before handling. The waiting was a little tough, but the end result was fantastic and well worth the wait. I would definitely recommend Caswell products. I liked this kit so much, that I am getting ready to order more.
-
First time user, Excellent results.
First time user. Excellent results. Thanks!
-
Great Product
The kit is great it works great for our parts, color is good and stays on. We'll be getting more.
-
Super Product
This Black Oxide Kit is just great. Have had this for some time and have done numerous items, from tools to firearms/parts. Good even blackening throughout. The penetrating sealer is just great.
-
Great product but prep is everything.
I have done a lot of parts with this product and been very happy with the results. I think any problems I have had were related to not getting the base metal clean enough. The good news is you can usually wipe it off, degrease it again and redo it and get a pretty even black. I had to redo a couple parts but I think I wan't careful enough prepping them. I also wash/soak the parts in hot water/defreaser which makes the process go very fast. A couple of minutes does the job. If you leave it on there longer you just end up wiping off a bunch of wasted black. It also helps a lot if you have baskets or something to dip the parts in the solution then remove and immediately rinse. Touching them with your fingers (even with gloves) seems to leave marks until you dunk them in the sealer.
-
this black oxide kit works great
I refinished 2 guns and multiple parts and i gotta say it works awesome hit it with wire wheel let it soak 5 minutes looks brand new.
-
Needed to darken some metal parts.
Excellent service. Recieved on time stated and product worked very well.
-
great, as always.
like all metal prep. matErials from caswell, the black oxide and sealer work great. thanks.
-
Kit worked as advertised
Very fast ship, Kit arrived complete. Kit worked as advertised. Would not hesitate to buy other Caswell products,
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.