Product Description
Blackens steel and iron parts (not stainless steel). Parts must be sealed after blackening. Use our Penetrating Sealer or Caswell Sealer.
Mix 1 part Concentrate with 9 parts distilled water. 1 quart of concentrate makes 2.5 gallons of blackening solution. Parts Coverage - 600 to 1200 sq. ft. of surface area blackened per gallon of concentrate.
Immerse the part in the mixed Black Oxide Solution and swirl around for between 30 seconds and 5 minutes. Alternatively, the part may simply be placed in the solution for 5 - 10 minutes. Remove the part from the solution and rinse in fresh water. Use at room temperature.
Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.
                
                    
                Recommended Skill Level
                    Beginner level products can and should be used by anybody, including those who consider themselves not crafty, handy or hands on. Most beginner level products can be used out of the box and can expect results within minutes. It is always important to read the product instructions and description on the web site before use, for example, nearly all of our plating kits require a polished and clean surface before plating.
Safety Information
Hazardous Shipping Info
GHS Info
SDS
Product Videos
Product Reviews
23 Reviews Hide Reviews Show Reviews
- 
                
Works really well. some tips and tricks
make sure you de-grease really well. Use Castrol de-greaser from Walmart (9/gal) and it works great full strength. Rinse in distilled H2O only. no tap water. Warm solution to 120 deg. F. it really helps. Remove and rise in distilled water. Coat with penetrating fluid for a more genuine look but is not the longest lasting solution. The Caswell sealer works really well and lasts long than oil. They say to dip in sealer immediately but i have rinsed with distilled H2O. Dried and used sealer with great results. Best of luck. This stuff works great.
 - 
                
The Best For Less
I'm a gunsmith and I use this a lots its a great product and will keep using it if the keep selling it and it is very easy to use and safe on the environment just make sure its clean.
 - 
                
Great Product Great Price
I'm a gunsmith and I used this on a couple of old and new guns that I was working on for customers and me and the customer was very very pleased, easy to use just be sure you get it clean and its very easy on the environment.
 - 
                
Only way to blacken automotive fasteners.
I have used this blackening solutition before and it works great. Just sandblast the part and put it in the solution then seal it.
 - 
                
Excellent Service
Very good product, leaves great finish
 - 
                
Excellent Service
Very good product, leaves great finish
 - 
                
Black Oxide Concentrate
Great product, and a great company to deal with. Will order from them again. Thanks
 - 
                
Good product slow service
Good product, slow service.
 - 
                
Works well and lasts a long time
I use this in a home based production environment to put a protective coating on the small brackets and parts I make for an Indy type race car.
 
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
 - Copper Wire to hang items
 - Small amount of electrical wire to make connections
 - DC Power Supply - Included In Some Kits. Check kit contents on web site
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
 - 1 Gal Battery Acid
 - Dyes (if desired)
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.