Product Description
Blackens steel and iron parts (not stainless steel). Parts must be sealed after blackening. Use our Penetrating Sealer or Caswell Sealer.
Mix 1 part Concentrate with 9 parts distilled water. 1 quart of concentrate makes 2.5 gallons of blackening solution. Parts Coverage - 600 to 1200 sq. ft. of surface area blackened per gallon of concentrate.
Immerse the part in the mixed Black Oxide Solution and swirl around for between 30 seconds and 5 minutes. Alternatively, the part may simply be placed in the solution for 5 - 10 minutes. Remove the part from the solution and rinse in fresh water. Use at room temperature.
Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.


Recommended Skill Level

Beginner level products can and should be used by anybody, including those who consider themselves not crafty, handy or hands on. Most beginner level products can be used out of the box and can expect results within minutes. It is always important to read the product instructions and description on the web site before use, for example, nearly all of our plating kits require a polished and clean surface before plating.
Safety Information
Hazardous Shipping Info

GHS Info


SDS
Product Videos
Product Reviews
23 Reviews Hide Reviews Show Reviews
-
quick and easy
I purchased the 5 gal kit for a specific project and hoped it would work and be enough to do all I needed. I have oxided several hundreds of machine brackets and have been extremely satisfied. I would recommend this to anybody that is looking for a quick easy way to make a profesional finish.
-
Use of the cold blue product
This product works well for its intended purpose. As with all metal finishing - preparation is the key.
-
Great results
Remarkable product, fast and easy to use. Did not realize black oxide could be this simple. Highly recommend this to anyone interested, 5 star rating.
-
this is a must
a wonderful product saves time and works fantastic. i have used this product many times and have had great results everytime
-
Plating and coating solutions
Just a pleasure to deal with ! ! The service has been really fantastic. Thanks
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.