Product Description
Blackens steel and iron parts (not stainless steel). Parts must be sealed after blackening. Use our Penetrating Sealer or Caswell Sealer.
Mix 1 part Concentrate with 9 parts distilled water. 1 pint of concentrate makes 1.25 gallons of blackening solution. Parts Coverage - 600 to 1200 sq. ft. of surface area blackened per gallon of concentrate.
Immerse the part in the mixed Black Oxide Solution and swirl around for between 30 seconds and 5 minutes. Alternatively, the part may simply be placed in the solution for 5 - 10 minutes. Remove the part from the solution and rinse in fresh water. Use at room temperature.
Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.


Recommended Skill Level

Beginner level products can and should be used by anybody, including those who consider themselves not crafty, handy or hands on. Most beginner level products can be used out of the box and can expect results within minutes. It is always important to read the product instructions and description on the web site before use, for example, nearly all of our plating kits require a polished and clean surface before plating.
Safety Information
Hazardous Shipping Info

GHS Info


SDS
Product Videos
Product Reviews
12 Reviews Hide Reviews Show Reviews
-
Great Product
Great Product
-
Love it!
I had been fighting rust on the machined surfaces in my shop (Table saw, drill presses, joiner etc) for years. just followed the easy instructions, problem solved. Great for machine parts, tools and anything steel. I found you can reuse your used dip solution for several days before it no longer works. Also be sure you rinse your items well and apply their sealer or light oil. Remington gun oil works well! Note: As much as we all love WD-40, don't use it for this, once the it has dried surface rust will start forming.
-
Excellent Product!
A very quick, easy to use process for short run parts! It is literally as simple as the instructions say and no big mess to worry about cleaning up.
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.