Product Description
1 Quart mixes with 2 gallons of water. Use to minimize smutting of aluminum parts before anodizing or plating. Use at 70-110 deg F, for 1-3 minutes.
Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.


Safety Information
Hazardous Shipping Info

GHS Info



SDS
Product Videos
Product Reviews
23 Reviews Hide Reviews Show Reviews
-
Super
Works great with little effort, cleans in seconds.
-
This is a MUST HAVE
This Deoxidizer/Desmut is a must have to eliminate the labor intensive cleaning process, and it does just that. Makes processing more fun.
-
exactly what it stated.
We needed some more deox/desmut and it came as described.
-
Shocked at the quality of this product!
Very impressed with this product, after stripping and cleaning my parts, they were dull and covered in smut, a few minuets in the deoxidizer/desmut and they were beautiful. Thanks! Worth every penny
-
Very good item to have
Helps to get items clean. De-anodizing sometimes leaves parts black and this product removes the black smut.
-
Good products
Good products and fast shipping
-
Great
Works as it should.
-
Key to success ?
As part of a system, I think that this is part of the reason for my successful outcomes with the anodizing process. Consistent results are so important.
-
Product as Advertised & Quick Delivery
Good product. Works good. This is my second purchase, so I would buy again from Caswell.
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.