Product Description
SOLDER-IT silver bearing solder paste in easy to use, no mess, no waste syringe. Soldering made easy - the skill is in the paste. Made from premium refined powdered metals. Ready to use - Flux is blended in, just add heat. No additional flux required. Works with the heat of a torch or soldering iron. Low melting point - flows smoothly at 430°F. Use with butane torch, soldering iron, propane, acetylene or map gas torch. Will join 22 different combinations of metals. 5 times as strong as ordinary solder. Finished joint is bright silver and won't tarnish or blacken. Great for electronics, wiring, connectors and circuit boards. Repairs copper, brass, bronze, nickel, platinum, chrome, coated steel, cast iron, black steel and steel. Stress and vibration resistant. Provides strength without the distortion of high temperature brazing. Extremely high electrical conductivity.
- No mess, no waste syringe
 - Works with the heat of torch or soldering iron
 - Ready to use - flux is blended in, no additional flux required- just add heat
 - Great for electronics - repairs copper, brass, bronze, nickel, platinum, chrome, Monel, coated steel, cast iron, black steel and steel
 - Low melting point - flows smoothly at 430°F, re-melts at 500°
 - Applications: wiring, connectors and circuit boards
 - Great for electronics
 - 7.1 gm lead-free solder and flux blended in easy to use syringe
 
            Safety Information
Product Videos
Product Reviews
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
 - Copper Wire to hang items
 - Small amount of electrical wire to make connections
 - DC Power Supply - Included In Some Kits. Check kit contents on web site
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
 - 1 Gal Battery Acid
 - Dyes (if desired)
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.