Product Description
Copper Conductive Paint
Make non-conductive items such as plastics, resins, leather, ceramics, cardboard, flowers, leaves, roses etc. conductive so they can be plated.
Copper Conductive Paint is an inexpensive alternative to our highly conductive Silvaspray™ silver conductive paint.
Porous items such as leather, cardboard, plants etc. should first be dipped in our Sealer Concentrate. Most plastics can be sprayed directly. No primer required.
Water based, latex paint. Non toxic and non hazardous. Can be thinned if desired with up to 6:1 water. Air dries in 1 hour. Coverage approx 20 sq ft per 4 fl oz.
It can be applied directly onto acrylic, ABS and structural foams, as well as solvent sensitive materials such as polycarbonate and polystyrene. It can be applied to almost any other non-porous surface, just use a latex primer first.
After spraying parts with the conductive paint, allow to dry and dip in Tinning Solution, then plate with our Acid Copper Plating Kit.
- Ideal for electroforming.
- Can be applied by sprayer, brush or roller just like ordinary latex paint!
- Good surface resistivity of <1 Ohm/sq at 1 mil dry film thickness. Attenuation: more than 75 dB from 30 MHz to 1.5 GHz.
- Dried coating is stable up to 250° F.
- Covers 670 ft² per gallon per mil thickness if application is 100% efficient
- RoHS Compliant.
- VOC: 1.0 ± 0.1 lbs/gallon (120.0 ± 12 grams/liter)
- Requires a small airbrush or Preval Sprayer.
- Available in 4oz and 1 Pint.
Safety Information
GHS Info
SDS
Product Videos
Product Reviews
11 Reviews Hide Reviews Show Reviews
-
Incredibly helpful customer service!
Very professional stuff that makes dealing with the company a pleasant experience.
-
easy product to use.
Either brushed on or sprayed the paint is easy to use and reacts easily to use.
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.