Product Description
Bronze & Blackening Solution
For use on Copper and Silver.
Mix 1-2 fluid oz of Concentrate to 1 gal water depending on degree of effect required. Use at room temperature. Dip item into solution for 5-10 seconds, longer for darker effect. Rinse to stop coloring effect.
Varying the solution strength and the time of immersion can produce an almost infinite range of shades.
For the €˜French Grey€™ effect on silver, scratch-brush or buff the high spots to expose the underlying silver. Add 1 fl oz Household ammonia to preserve the mixed solution.
|  |  |  |  | 
| Brassy Bronze (1 second                                    dip)(very iridescent) | Light Japanese bronze (3                                    seconds dip) | Statuary bronze (10 20                                    second dip) | Dark purple (30 seconds                                     2 mins) | 
|  | |||
| Black (2-10                                    minutes) | |||
|  | 
 
                Recommended Skill Level
 
                    Beginner level products can and should be used by anybody, including those who consider themselves not crafty, handy or hands on. Most beginner level products can be used out of the box and can expect results within minutes. It is always important to read the product instructions and description on the web site before use, for example, nearly all of our plating kits require a polished and clean surface before plating.
Safety Information
Hazardous Shipping Info
 
  			 GHS Info
 
			  
			 Product Videos
Product Reviews
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
- Copper Wire to hang items
- Small amount of electrical wire to make connections
- DC Power Supply - Included In Some Kits. Check kit contents on web site
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
- 1 Gal Battery Acid
- Dyes (if desired)
- Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
- Other minor household items may be required, such as gloves, water etc.
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.
 
 
             
             
           
       
            