Caswell Brass Plating Solution is a unique cyanide-free alkaline brass plating system which plates a true 70/30 yellow-green plate directly onto steel and bright nickel plated surfaces. It can be used for heavy brass plating which will be antiqued (oxidized and relieved). It may also be used for decorative heavy brass if the surface is burnished or buffed and colored with a wheel to remove the slight haze and reveal the true rich brass color for lamp parts, hardware and plumbing fixtures.
To plate on zinc die cast surfaces, you must plate with Flash Copper™ first.
The system eliminates carbonates. Therefore, there is no carbonate sludge containing cyanide to be disposed of.
The solution may be used to tank or brush plate.
Brass tank plating requires an average current of 0.02-0.1 amps per sq. in. and operates in the range of 3-12 Volts. 
Brass Plating is available on a small scale using Plug N' plate kits.

1 Gallon Kit Contains:
- 1 x 2 Gal Tank and Lid
 - 2 x Brass Anodes (4" x 8")
 - 4 Quarts Brass Solution Part A
 - 2 x 4oz Brass Solution Part B
 - The Caswell Plating Manual
 - Free Technical Support
 - NO HEATERS INCLUDED
 
Contains Hazardous Goods. Shipping restrictions apply. Ground shipping only to the Continental USA. Please call +1 315 946 1213 or contact us for rates to other locations.

                Recommended Skill Level
                    Intermediate level products require some extra work before use, or multiple steps to achieve end results. Intermediate level products can certainly be used by novices, but extra time, patience and research will greatly help get great results.
Safety Information
Hazardous Shipping Info
GHS Info
SDS
Product Videos
Product Reviews
2 Reviews Hide Reviews Show Reviews
- 
                
great set up
I have this kit in my shop works good I have had others in the past but this set up is easy to use and has everything to get started , highly recommended
 - 
                
workes great
This kit made it easy to plate my antique hinges they look great very happy with this kit
 
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
 - Copper Wire to hang items
 - Small amount of electrical wire to make connections
 - DC Power Supply - Included In Some Kits. Check kit contents on web site
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
 - 1 Gal Battery Acid
 - Dyes (if desired)
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.