Product Description
Black Krome™ Kit

This spectacular product will add style and elegance to many products. Safe to use. Contains no chrome or nickel.
Ideal for vehicle trim, guns, musical instruments, fishing lures, etc.
The system plates within a couple of minutes over a nickel or copper base. To plate over chrome, the existing chrome plate must be removed by stripping with Anodize & Chrome Stripper.
Black Krome™ can be plated by brush plating or by an immersion technique.
Black Krome will plate over Nickel, Copper, Steel, Tin & Lead.
For brush plating, a 4.5 volt power supply and a stainless steel wand is required. Immersion plating requires 0.24 amps per square inch at 3-7V.
For tank (immersion) plating, the solution is best used at 140 deg f, using a stainless steel anode. Because the plate is derived from the solution and not the anode, the solution will need to be replaced periodically.
When plating over nickel, the color will have a metallic smoky black look, whereas over copper, a darker black will be achieved.
The finish should be waxed with Collinite Insulator or Metal Wax, or clearcoated.

2 Gallon Kit Contains
- 1 x 3.5 Gal Tank and Lid
 - 2 x Stainless Steel Anode
 - 2 Gal Black Krome™ Solution
 - Caswell Plating Manual
 - Free Technical Support
 - NO HEATERS INCLUDED
 
                Recommended Skill Level
                    Intermediate level products require some extra work before use, or multiple steps to achieve end results. Intermediate level products can certainly be used by novices, but extra time, patience and research will greatly help get great results.
Safety Information
SDS
Product Videos
Product Reviews
5 Reviews Hide Reviews Show Reviews
- 
                
Super product
I got this kit to do some custom plating for a couple of my projects that I wanted to put a dark shine on. Like the other Caswell kits I have gotten this one arrived quickly, was well packaged, and was very easy to set up and use. For those of us who do home art work or restorations, these Caswell kits have been a huge help to my business. They allow me to do the work as I want, when I want, without the hassle of having to ship parts out and hope they turned out the way I wanted.
 - 
                
awesome kit
Looks great on my bike and will buy again....
 - 
                
nice kit
Works great, very nice look and was not that hard to do
 - 
                
wroks
A happy wife is a happy life, this kit is great and was easy to do
 - 
                
Worked Great.
Another fine product from Caswell. I ve been using Caswell's Black Krome kit for years with great success. Just have to make sure your product is 100% clean before plating as the Black Krome must have perfect settings to work properly.
 
Important Information
Additional Equipment May Be Required
For Our Tank Plating Kits:
- Copper Pipe for tank bar
 - Copper Wire to hang items
 - Small amount of electrical wire to make connections
 - DC Power Supply - Included In Some Kits. Check kit contents on web site
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
For Our Anodizing Kits:
- DC Power Supply (Standard Kit Only)
 - 1 Gal Battery Acid
 - Dyes (if desired)
 - Optional Rinse Tanks (or rinse over the plating tanks with a water bottle)
 - Other minor household items may be required, such as gloves, water etc.
 
Learn More Before Buying
You can purchase our Caswell Plating Manual and learn how to use the kits, before purchasing a kit. Simply Order Here. When you are ready to buy, we will discount the price of the kit.
Already Have Our Plating Manual?
If you are ordering a plating kit that contains our Plating Manual, and you already have our Plating Manual, you can remove it from all kits that contain it and save $30 per kit. Just use Coupon Code NOMANUAL in your Shopping Cart at checkout.