null

We are experiencing delays with some products due to supply chain and shipping carrier delays. All delivery date guarantees are cancelled. Please plan accordingly.

Black Oxide Kits

  • BLACK OXIDE CONCENTRATE 1 PINT

    BLACK OXIDE CONCENTRATE 1 PINT

    Blackens steel and iron parts (not stainless steel). Parts must be sealed after blackening. Use our Penetrating Sealer or Caswell Sealer. Mix 1 part Concentrate with 9 parts distilled water. 1 pint of concentrate makes 1.25 gallons of blackening...
    $31.89
    Add to Cart
  • Black Oxide Kit - 1.25 Gal Black Oxide Kit - 1.25 Gal

    Black Oxide Kit - 1.25 Gal

    Blacken Steel Or Iron Parts At Room Temperature This new technique was developed by the commercial gun blue manufacturers as a more environmentally friendly system than the commonly used hot application. Parts requiring blackening are simply placed in...
    $76.99
    Choose Options
  • BLACK OXIDE CONCENTRATE 1 QT

    BLACK OXIDE CONCENTRATE 1 QT

    Blackens steel and iron parts (not stainless steel). Parts must be sealed after blackening. Use our Penetrating Sealer or Caswell Sealer. Mix 1 part Concentrate with 9 parts distilled water. 1 quart of concentrate makes 2.5 gallons of blackening...
    $52.79
    Add to Cart
  • Black Oxide Kit - 2.5 Gal Black Oxide Kit - 2.5 Gal

    Black Oxide Kit - 2.5 Gal

    Blacken Steel & Iron Parts At Room Temperature This new technique was developed by the commercial gun blue manufacturers as a more environmentally friendly system than the commonly used hot application. Parts requiring blackening are simply placed in...
    $141.90
    Choose Options
  • Black Oxide Concentrate - 1 Gallon

    Black Oxide Concentrate - 1 Gallon

    Blackens steel and iron parts (not stainless steel). Parts must be sealed after blackening. Use our Penetrating Sealer or Caswell Sealer. Mix 1 part Concentrate with 9 parts distilled water. 1 gallon of concentrate makes 10 gallons of blackening...
    $196.90
    Add to Cart
  • Caswell Mega Black™ Kit Caswell Mega Black™ Kit

    Caswell Mega Black™ Kit

    Caswell Mega Black™ Blackening Kit Deeper, Darker FinishCan Be Shipped Worldwide and by AirRoom Temperature Blackening Of SteelNo Dangerous Fumes Or Corrosive Chemicals   Our NEW Caswell Mega Black™ is the most advanced blackening...
    $130.90
    Choose Options
  • BLACK OXIDE CONCENTRATE 5 GAL

    BLACK OXIDE CONCENTRATE 5 GAL

    Blackens steel and iron parts (not stainless steel). Parts must be sealed after blackening. Use our Penetrating Sealer or Caswell Sealer. Mix 1 part Concentrate with 9 parts distilled water. 5 gallons of concentrate makes 45 gallons of blackening...
    $658.90
    Add to Cart
  • Black Oxide Kit - 5 Gal

    Black Oxide Kit - 5 Gal

    Blacken Steel & Iron Parts At Room Temperature This new technique was developed by the commercial gun blue manufacturers as a more environmentally friendly system than the commonly used hot application. Parts requiring blackening are simply placed in...
    $241.99
    Choose Options
  • Heat Coloring Kit For Steel & Stainless Steel

    Heat Coloring Kit For Steel & Stainless Steel

    Color steel and stainless steel parts by heat treating and oil quenching Possible colors include yellows, browns, purples and blues. Our Heat Coloring Kit Includes Casweld™ Keep Kool™ Putty, which prevents heat from travelling up your pliers or other...
    $54.99
    Add to Cart