Dupli-Color Mirage System
These unique paints have been formulated to create
multi-colored effects from all angles. As the light
source and viewing angle changes, the color appears
to change. Designed to work as an easy-to-apply, three-step
system, the base coat, mid-coat, and top coat work
together to create dramatic color effects in a durable,
high-gloss finish.
MIRAGE® Color Kit
Complete MIRAGE® Color Kit includes everything
you need to create dazzling color shifting effects.
Kit includes 1 can of Black Base Coat, 1 Can of Mid-Coat,
and 1 can of Clear Top Coat. Kits available in 5 color
shifting combinations: Purple/Green, Silver/Green,
Gold/Magenta, Red/Blue and NEW Ice, a radiant silver
color with brilliant rainbow highlights.
MIRAGE® Black Base Coat
Exclusively formulated to provide an even black lacquer
base coat. It gives a smooth finish that's the essential
first step to creating the desired color "shifting" effect.
MIRAGE® Mid-Coat Color
This exclusive, high-quality acrylic lacquer changes
color depending on light, angle, and surface contour.
It can be used on cars, trucks, bikes, helmets, skateboards,
and other applications where dramatic color changes
are desired.
MIRAGE® Top Coat Clear
Designed to provide protection and shine, this durable
high-gloss clear lacquer is the perfect topcoat for
MIRAGE® color shifting paint.

Gold/Magenta |

Purple/Green |

Blue/Red |

Ice
|

Silver/Green |
|