The special gun is attached to an air compressor, and
a power unit. The air blows the powder from the gun,
and the power unit gives the powder a positive charge.
At the same time, the power unit is connected to the
piece being coated, and so it has a negative charge.
As the positive paint particles fly through the air,
they are attracted to the part and lay in an even layer
over the entire area of the part. (This works a little
like dust on a TV screen.)
The part is then placed in an dedicated
electric oven, and baked for a while. This cures the
coating to a tough chemical resistant finish.
It is important not to use a gas oven, as the emissions
from the coating are flammable.
The moisture filter must be changed regularly to ensure best operation.
Why are our powder guns better
than our competitors?
- Our powders cups are tapered to provide smoother
flow, and they are gravity fed, rather than siphoned.
- The charge switch is controlled by a foot pedal,
leaving your hands free - competitor's are hand controlled.
- The power pack is more compact and lighter.
- Sturdier construction - less powder leaks
- Works with any manufacturers virgin powder
coating. Do not use reclaimed powder.
Now Includes 1
Pound Of Super Wet
Black Powder Coating

Courtesy myillwillinc
- 30 Day Limited Warranty
- Input Voltage: 110volt 60HZ
AC
- Air Requirement: 15PSI @ 5 CFM
- Fixed Output Voltage: 16KVDC
- Manual Discharge
- 2 x Powder Gun Cups
- 3 x Conical Fan Spray Pattern
tips
- External High Voltage Power
Supply
- In line disposable filter
- Foot switch
- Ground Clip Cable
- Free Technical Support
- 1 lb Super Wet Black Powder
Coating
|
|
|