Caswell Inc Sells Plating Kits - Electroplating Kits - Anodizing - Powder Coating and Metal Polishing Supplies
 
USA Customers Canada Customers UK and European Customers UK and European Customers Australia & New Zealand Customers Rest Of World
View Shopping Cart Login To Your Account Get Help Using Our Web Site
Caswell Inc. Home Page Plating Kits, Anodizing Kits, Chrome, Nickel, Gold, Zinc Buffing Wheels, Kits, Compound and Machines Wax, Polish, Lacquer, Epoxies & Specialized Repair Powder Coating Systems, Powder Coating, Ceramic, Ovens VHT, Krylon, Permatex Products Radio Controlled Models and Supplies Special Offers and Clearance Items
 
Home > Buffing Supplies > ZoopSeal
Search Caswell Inc.

Web Site Features
Start Here

Customer Gallery

Customer Testimonials

Technical Support

Finishing Forum

Online Manual

Free Catalog

Free How To Buff & Polish Booklet

Videos & Tutorials


More Tools
Join Our E-Mail List

Recent Forum Postings

Recent News

British Tools and Fasteners

Contact Caswell

Join Our Affiliate Program To Earn 15% of Referred Sales

ZoopSeal™

From Zoops Products

ZoopSeal

Protect all your polished aluminum, stainless steel and chrome parts from oxidation and eliminate the need for repeat polishing. A kit covers 75 square feet. Easy to apply when following the instructions provided. Formulated for use on cars, trucks, boats motorcycles, engines, wheels and interior accessories. When applied properly ZoopSeal™ will:

Applications Of This Product
  • A hybrid ceramic sealer that protects finishes for up to two years.

Related Products

  • Prevent dulling and oxidation
  • Retain the polished brightness and luster of aluminum
  • Eliminate the need for repeat polishing
  • Be long lasting
  • Will work on aluminum, brass, and stainless steel
  • Be safe to use and environmentally friendly
Without ZoopSeal
With ZoopSeal
Without ZoopSeal
With ZoopSeal

Kit Contains:

  • Zoops Cleaner Concentrate
  • ZoopSeal Part A
  • ZoopSeal Part B
  • Final Sealer
  • Spray Bottle
  • Written Instructions
  • Application Cloths
  • Rubber Gloves


This kit will supply you complete coverage for 75 sq. ft, which covers an entire engine AND four wheels. ZoopSeal will NOT remove any scratches or nicks that are on your product, so you may need to have your product re-polished BEFORE you apply ZoopSeal, since it will seal in any defects your product already has.

Pre-Application Step:

Pour the bottle Part “B” into the bottle Part “A”, (DO NOT USE ANOTHER BOTTLE YOU MAY HAVE laying around, we provide you with all bottles). Shake the bottle to mix it together. This becomes ZoopSeal, the mixture could take a max. 3 hours to complete the blending process. Periodically shake the bottle up. (If mixture looks separated after you continue to shake the bottle, please call ZoopSeal). WARNING: PART “A” AND PART “B” ARE FLAMMABLE! DO NOT SMOKE OR LIGHT A MATCH AROUND THESE CHEMICALS! ZoopSeal is not compatible with strong acids and alkaline products. These will remove the ZoopSeal.

Application Steps:

STEP 1:

ZoopSeal Concentrate Cleaner

  1. Clean product thoroughly with ZoopSeal cleaner, you can use the towels provided or a soft lint free polishing cloth.
  2. Mix ZoopSeal Cleaner: 15 parts tap water to 1 part ZoopSeal cleaner in the 8 oz. spray bottle included in the kit.
  3. Spray ZoopSeal Cleaner onto product and thoroughly clean the product. You may repeat this process as many times as you need in order to have a “squeaky” clean product. Be sure to rinse the product off each time with distilled water.
  4. Make sure the product is “squeaky” clean and free of streaking or water spotting. No water droplets left , water and ZoopSeal do not mix. The product being treated needs to be completely dry.

STEP 2:

ZoopSealer (Product left over needs to be refrigerated. It should last up to 2 weeks, refrigerated.)

  1. Take the pre-mixed ZoopSealer and apply it in a dry environment. Apply a small amount onto a lint free soft polishing cloth. Only swipe ZoopSeal on in one direction one time, until the product is completely covered. DO NOT RUB ZoopSeal into your product, ZoopSeal automatically flows into the pores of the product. A transparent, rainbowed film will appear, this is normal. Do not apply ZoopSeal too heavily. More is NOT better*!
  2. Allow ZoopSeal to become dry to the touch. This could be as little as two hours and up to 24 hours. For Polished parts - proceed to step 3 below; un-polished parts are sealed and do not need step 3.* If ZoopSeal is applied too heavily, a more aggressive finish polish will have to be used to remove the excess. We suggest the use of an aggressive billet aluminum polish to remove this excess. We then advise to use Zoops Final Seal after the removal of the excess.

STEP 3:

Zoops Final Seal** (do not allow zoops final seal to dry on your product!)

  1. Apply lightly with 3” square towel in sections of 6” x 6”.
  2. While Final Seal is still wet start polishing off the product where ZoopSeal has been applied, using back and forth strokes until the Final Seal is no longer visible and a luster appears. If needed, Final Seal can be applied several times using the same back and forth strokes in order to produce the shine on your product.
  3. Allow coated material to cure in a warm dry place for 24 hours.
    **Do Not apply Final Seal to NON-POLISHED parts. It is for use on polished parts ONLY

Not ready to use all 4 ounces of ZoopSeal? Mix 3⁄4 of 1 ounce of Part “A” to 1⁄4 of 1 ounce Part “B” EXACTLY.

What is Zoopseal?
Zoopseal is a hybrid ceramic sealer, it is not a polish or wax. It is a protectorate.
What does a ceramic base sealer do?
It will impregnate into the pores of the product being treated, which will stop the process of oxidation immediately. A crisp, and clean appearance is the end result. Your product will continue to look like new without repolishing.
What can I use Zoopseal on?
Aluminum, Raw Aluminum, Brass, Chromed Plating, Stainless Steel, Anodized Aluminum Parts, Stainless Steel in Restaurant Kitchens, Outside Furniture, Awnings, and Paint.
How long does Zoopseal last on my product?
2 to 3 years.
When it is time to re-apply after 2 to 3 years, how and what are the steps?
You will need to re-condition your product if necessary and re-apply (you’ll need to re-order a Zoopseal Kit) using the same method as before. Just follow the Kit instructions and your product will continue to look like new.
Will Zoopseal rejuvenate or refurbish my product?
No, it will not. It will only protect from oxidation and dulling.
Will it harm the painted finishes on my car?
No it will not.
Will Zoopseal provide protection against fresh water?
Yes, but not against underwater abrasions.
What does salt water do to Zoopseal?
We recommend that you do not have your product immerged into salt water for a length of time (over 2 hours). If exposed to salt water use soapy water and wash off the salt within 2 hours. Salt water will cause your product to discolor.
How can I get Zoopseal off my product once it is applied?
By repolishing the product using any commercial polish.
What type of cleaners can be used on Zoopseal?
NO CAUSTIC OR ALKALINE CLEANERS. Only Zoops Cleaner is to be used on the product.
How much Zoopseal do I need on the lint free towel during the application process?
Very little!!! The towel should be barely damp, NOT WET!
Can I use Zoopseal on my radiator and will heat affect it?
Yes, you can use Zoopseal on a radiator. Heat from the radiator will help it to cure and make it stronger. We do not recommend putting Zoopseal on an exhaust, this heats up too much.
Can I use Zoopseal on Magnesium?
No, not yet, it is still being tested.
Can I use Zoopseal on Copper?
No, this has been tested.
Can I use Zoopseal on Fiberglass?
No, not yet, it is still being tested.

Quantity Product Code Name   Price  
ZSEAL ZoopSeal Kit $129.95
Not Hazardous
ZSEALMINI ZoopSeal Mini Kit (covers 35 sq ft) $99.95
Not Hazardous
       
       
Not Hazardous - Not Hazardous Goods. Ship By Air if Desired.
No Air Shipping - ORM-D Product. No Air Shipping. Click Picture For Details.
Hazardous Goods - HAZMAT Product. HAZMAT Fee Applies. No Air Shipping. Click Picture For Details.
   
Login or Email
Password
Lost Password?
Create An Account